Material wise Lower and upper temp Limitation
back
| Material | Lower(F) | Upper (F) |
| Cast Iron | -20 | 410 |
| Ductile Iron | -20 | 650 |
| *Carbon Steel (Grade WCB) | -20 | 1000 |
| Carbon Steel (Grade LCB) | -50 | 650 |
| Carbon Moly (Grade WC1) | -20 | 850 |
| 1-1/4 Cr - 1/2 Mo (Grade WC6) | -20 | 1000 |
| 2-1/4 Cr - 1 Mo (Grade WC9) | -20 | 1050 |
| 5 Cr - 1/2 Mo (Grade C5) | -20 | 1100 |
| 9 Cr - 1 Mo (Grade C12) | -20 | 1100 |
| Type 304 (Grade CF 8) | -425 | 1500 |
| Type 347 (Grade CF8C) | -425 | 1500 |
| Type 316 (Grade CF8M) | -425 | 1500 |
| 3-1/2 Ni (Grade LC3) | -150 | 650 |
| Aluminum | -325 | 400 |
| Bronze | -325 | 550 |
| Inconel | 600 -325 | 1200 |
| Monel 400 | -325 | 900 |
| Hastelloy B | -325 | 700 |
| Hastelloy C | -325 | 1000 |
| Titanium | 600 | |
| Nickel | -325 | 500 |
| Alloy 20 | -50 | 300 |